PP
사양
직경:
무게:

파라미터 정보
| Mechanical Properties | Physical Properties | Print Settings | |||
|---|---|---|---|---|---|
| Tensile Strength(MPa) | 19±3 | Density(g/cm³) | / | Nozzle Temperature & Print Speed | 210-230℃ / ≤30mm/s |
| Flexural Strength(MPa) | 19±3 | Melt Flow Index(g/10 min) | 9.75±2 | Bed Temperature | 50-60℃ |
| Notched Izod Impact Strength(kJ/㎡) | 5.3±1.5 | Shrinkage(%) | 1.5 | Retraction Distance | 0.8-1.2mm |
| Elongation at Break(%) | 850±150 | Heat Deflection Temperature(℃) | 58.5±3 | Retraction Speed | 30-40mm/s |
| Shore Hardness(HA/HD) | 54.5 | Vicat Softening Temperature(℃) | / | ||