PLA Wood
SUNLU wood PLA filament contains 15% wood powder, producing prints with a natural wood-like appearance and scent. It serves as a popular wood-infused PLA filament for models and decorative items that call for a warm, organic finish.
Diameter:
Weight:


Contains 15% wood powder, producing prints with wood texture and aroma
SUNLU wood-infused PLA filament displays natural wood grain textures, offering a realistic touch and a subtle wood scent. This PLA wood filament adds a natural feel and artistic flair to every model.

Supports high-speed printing up to 400 mm/s, greatly improving efficiency
SUNLU wood filament PLA effectively reduces print time and significantly improves printing efficiency, meeting the demands of high-efficiency production and rapid prototyping for every 3D wood filament PLA project.

Neat filament winding reduces tangling and nozzle clogging risk
SUNLU filament PLA wood is produced using a neat winding process, with tightly and orderly arranged strands that effectively reduce tangling and knotting, lowering the risk of clogging from the source and ensuring a stable and smooth high-speed printing process.
Parameter Information
| Mechanical Properties | Physical Properties | Print Settings | |||
|---|---|---|---|---|---|
| Tensile Strength(MPa) | 33±6 | Density(g/cm³) | 1.17 | Nozzle Temperature & Print Speed | 200-220℃ / ≤230mm/s |
| Flexural Strength(MPa) | 55±5 | Melt Flow Index(g/10 min) | 3.8±1.5 | Bed Temperature | 50-60℃ |
| Notched Izod Impact Strength(kJ/m²) | 6±3 | Shrinkage(%) | 0.1-0.3 | Retraction Distance | 0.8-1.2mm |
| Elongation at Break(%) | 10±5 | Heat Deflection Temperature(℃) | 55±3 | Retraction Speed | 30-40mm/s |
| Shore Hardness(HA/HD) | 77 | Vicat Softening Temperature(℃) | 54 | ||
Color Code
| Color | Hex Code | Display |
|---|---|---|
| Wood | #997D73 | ![]() |
| Maple wood | #E5BD8E | ![]() |
| Walnut wood | #58473F | ![]() |
| Cherry wood | #AC7575 | ![]() |